Law , K A , Parry , S A , Bryan , N D , Heath , S L , Heald , S , Knight , D , O'Brien , L , Fuller , A J , Bower , W R , Law , G T W & Livens , F R 2019 , ' Plutonium Migration during the Leaching of Cemented Radioactive Waste Sludges ' , Geosciences , vol. 9 , no. 1 , 31 . https://doi.org/10.3390/geosciences9010031

Title: Plutonium Migration during the Leaching of Cemented Radioactive Waste Sludges
Author: Law, Kathleen A.; Parry, Stephen A.; Bryan, Nicholas D.; Heath, Sarah L.; Heald, Steven; Knight, Darrell; O'Brien, Luke; Fuller, Adam J.; Bower, William R.; Law, Gareth T. W.; Livens, Francis R.
Other contributor: University of Helsinki, Department
University of Helsinki, Department of Chemistry

Date: 2019-01-08
Language: eng
Number of pages: 13
Belongs to series: Geosciences
ISSN: 2076-3263
DOI: https://doi.org/10.3390/geosciences9010031
URI: http://hdl.handle.net/10138/303579
Abstract: One of the most challenging components of the UK nuclear legacy is Magnox sludge, arising from the corrosion of Mg alloy-clad irradiated metallic U fuel that has been stored in high pH ponds. The sludges mainly comprise Mg hydroxide and carbonate phases, contaminated with fission products and actinides, including Pu. Cementation and deep geological disposal is one option for the long-term management of this material, but there is a need to understand how Pu may be leached from the waste, if it is exposed to groundwater. Here, we show that cemented Mg(OH)2 powder prepared with Pu(IV)aq is altered on contact with water to produce a visibly altered ‘leached zone’, which penetrates several hundred microns into the sample. In turn, this zone shows slow leaching of Pu, with long-term leaching rates between 1.8–4.4 × 10−5% of total Pu per day. Synchrotron micro-focus X-ray fluorescence mapping identified decreased Pu concentration within the ‘leached zone’. A comparison of micro-focus X-ray absorption spectroscopy (μ-XAS) spectra collected across both leached and unleached samples showed little variation, and indicated that Pu was present in a similar oxidation state and coordination environment. Fitting of the XANES spectra between single oxidation state standards and EXAFS modeling showed that Pu was present as a mixture of Pu(IV) and Pu(V). The change in Pu oxidation from the stock solution suggests that partial Pu oxidation occurred during sample ageing. Similarity in the XAS spectra from all samples, with different local chemistries, indicated that the Pu oxidation state was not perturbed by macro-scale variations in cement chemistry, surface oxidation, sample aging, or the leaching treatment. These experiments have demonstrated the potential for leaching of Pu from cementitious waste forms, and its underlying significance requires further investigation.
Subject: 116 Chemical sciences
114 Physical sciences
plutonium
radioactive waste
speciation
cement
leaching
SPECIATION
Rights:


Files in this item

Total number of downloads: Loading...

Files Size Format View
geosciences_09_00031.pdf 3.058Mb PDF View/Open

This item appears in the following Collection(s)

Show full item record