Effect of porogen solvent on the synthesis of nickel ion imprinted polymer materials prepared by inverse suspension polymerization

Näytä kaikki kuvailutiedot



Pysyväisosoite

http://hdl.handle.net/10138/310027

Lähdeviite

Meouche , W , Laatikainen , K , Margaillan , A , Silvonen , T , Siren , H , Sainio , T , Beurroies , I , Denoyel , R & Branger , C 2017 , ' Effect of porogen solvent on the synthesis of nickel ion imprinted polymer materials prepared by inverse suspension polymerization ' , European Polymer Journal , vol. 87 , pp. 124-135 . https://doi.org/10.1016/j.eurpolymj.2016.12.022

Julkaisun nimi: Effect of porogen solvent on the synthesis of nickel ion imprinted polymer materials prepared by inverse suspension polymerization
Tekijä: Meouche, Walid; Laatikainen, Katri; Margaillan, Andre; Silvonen, Timka; Siren, Heli; Sainio, Tuomo; Beurroies, Isabelle; Denoyel, Renaud; Branger, Catherine
Tekijän organisaatio: Department of Chemistry
University Management
Päiväys: 2017-02
Kieli: eng
Sivumäärä: 12
Kuuluu julkaisusarjaan: European Polymer Journal
ISSN: 0014-3057
DOI-tunniste: https://doi.org/10.1016/j.eurpolymj.2016.12.022
URI: http://hdl.handle.net/10138/310027
Tiivistelmä: Ion-imprinted polymers (IIPs) for nickel were synthesized by inverse suspension copoly-merization of vinylbenzyl iminodiacetic acid (VbIDA) with ethyleneglycol dimethacrylate (EDMA) in the presence of nickel(II) ions with various porogen solvents to study their impact on the IIPs properties. They were prepared with mixtures of acetonitrile and dimethylsulfoxide (DMSO), 50/50%v/v, for IIP-A/D and 2-methoxyethanol and DMSO, 50/50%v/v, for IIP-M/D. The structure and properties of these polymers were compared with those of IIP-D previously prepared with pure DMSO as porogen solvent. Although IIP-A/D and IIP-M/D were less porous than IIP-D, they presented better nickel adsorption properties and selectivity towards Zn2+, Co2+ and Pb2+. This is assumed to be the result of the stabilization of the ligand-metal complex during the polymerization process. Moreover, the nickel binding capacities of the prepared IIPs in competitive conditions are remarkably high (184 mu mol/g for IIP-D, 170 mu mol/g for IIP-A/D and 174 mu mol/g for IIP-M/D). The impact of the VbIDA chelating monomer was highlighted by comparing the adsorption properties of a copolymer of methyl methacrylate (MMA) and EDMA with NIP-D. It was proved that the methacrylic polymer matrix has low binding properties. (C) 2016 Elsevier Ltd. All rights reserved.
Avainsanat: 116 Chemical sciences
Ion-imprinted polymer
Inverse suspension polymerization
Porogen
Nickel
Selective adsorption
Vertaisarvioitu: Kyllä
Pääsyrajoitteet: openAccess
Rinnakkaistallennettu versio: acceptedVersion


Tiedostot

Latausmäärä yhteensä: Ladataan...

Tiedosto(t) Koko Formaatti Näytä
List_number_10_manuscript_Article_MMM_v4b.pdf 1.299MB PDF Avaa tiedosto

Viite kuuluu kokoelmiin:

Näytä kaikki kuvailutiedot